Salt on the harbour side and what it does to VELUX flashing zinc

Flashing metal, not the window, is what fails first on a salt-exposed roof, and the mechanism differs between the open spit and the sheltered harbour side.

A roof window set between rafters in a pitched coveringThe window sits in the plane of the covering between existing rafters. A flashing kit matched to the covering carries water around the frame, and the underlay is dressed to a collar so anything passing the tiles is returned to the outside.roof windowrafterrafterflashing kitcovering

On a coastal roof the flashing outlives its warranty or it does not, and the difference is metallurgy rather than workmanship. The window will usually still be sound when the metal round it has gone.

This guide is about the metal, not about choosing between flashing families. Which kit suits which covering is settled in our guide to matching a flashing to the roof covering; what follows is what happens to that kit once it is up there, a few hundred metres from open water, and how the answer changes between Sandbanks and Lower Parkstone.

What a flashing is actually made of

A roof window flashing is a set of pressed metal sections. The apron, the side sections and the head section are aluminium, mill-finished or coated. The soakers and the pieces that interleave with the covering are frequently zinc or a zinc-coated steel. The fixings are a separate metal again, and the clips that hold the sections together another.

That is four metals sitting in permanent contact, outdoors, wetted several times a week. Inland this is uneventful. On the water it is a chemistry set.

Two mechanisms, and they are not the same thing

Mechanism What is happening Where it shows first What slows it
Chloride attack Airborne salt holds moisture on the surface long after rain has stopped, keeping the metal wet for hours a day Flat and sheltered faces where water sits: the apron, the underside of laps Rain washing, a coating, and surfaces that drain rather than pool
Galvanic action Two dissimilar metals in contact with a salt film between them form a cell, and the less noble one sacrifices itself Around fixings, clips and any steel screw driven through aluminium or zinc Matching the fixing metal to the flashing, or isolating them

Most homeowners have heard of the first. It is the second that quietly does the damage, because it concentrates at a handful of points instead of spreading evenly, and a flashing can lose its grip at four fixings while the rest of it still looks new.

Why the spit is a different problem from the harbour side

Salt deposition is not a function of distance from the sea. It is a function of how far the wind has travelled over open water before it reaches you, and whether anything broke it on the way.

Where The exposure What we expect of the metal
Sandbanks, Studland, Mudeford Water on both sides, no fetch break at all, salt arriving as spray as well as aerosol Coated aluminium, stainless fixings throughout, no bare zinc in a wetted lap
Hamworthy, Lower Parkstone, Upton Salt present, but the prevailing south-westerly has crossed land first and dropped most of its load Coated aluminium, stainless fixings, standard kit otherwise fine
Southbourne, Boscombe, Highcliffe Genuine salt load with the land behind giving partial shelter As above, with a shorter inspection interval on south-west elevations
Broadstone, Creekmoor, Wimborne Heathland edge, effectively inland Standard specification. Marine-grade here is money spent on nothing

The fixing that eats the flashing

The single most common coastal failure we open up

A plated steel screw through an aluminium apron. The plating survives three or four winters. After that the steel is exposed, the salt film bridges it to the aluminium, and the aluminium round the hole corrodes away in a ring. The screw stays; the metal it was holding tears.

Why it happens: the screws that came in the box got lost, or a second window went in and somebody used what was in the van. It is not a specification decision. It is a five-minute decision made on a roof in the wind.

What we do instead: austenitic stainless fixings on everything within sight of open water, and the supplied fixings never substituted. On the spit that extends to the battens and the clips, not just the visible screws.

Salt on the harbour side and what it does to VELUX flashing zinc
The kerb is measured before anything is ordered.

Reading a flashing that is already twenty years old

Corrosion on a roof window surround goes through recognisable stages, and knowing which one you are looking at is the difference between a wash and a re-flash.

Stage What you see What it means
White bloom A chalky grey-white film on the aluminium, wipes partly off Surface oxide doing its job. Cosmetic. Wash it and leave it
Pitting Small dark craters, gritty under a fingernail Chloride has broken through the oxide locally. Watch it, shorten the interval
Rings at fixings Corrosion haloes round screw heads, sometimes rust staining down the apron Galvanic. The joint is losing its hold. Fixings out and replaced before the metal tears
Perforation or lifted lap Daylight through the metal, or a lap standing proud of the covering The weather line is gone. Re-flash, regardless of how the window looks

Washing is corrosion control, not cleaning

Rainwater washes salt off the faces it reaches. It does not reach the underside of laps, the sheltered back of the head section, or the pocket where the apron meets the tile course. Those are precisely the places chloride accumulates, because they get wetted by aerosol and never rinsed.

Twice a year on the spit, a bucket of fresh water over the flashing perimeter does more for its life than any product sold for the purpose. It wants to be plain water. Detergents leave a residue that holds moisture, and anything acidic strips the coating you are trying to protect.

The soakers matter more than the visible metal. The sections you can see from the garden are coated aluminium and behave well. The pieces that interleave with the tiles are frequently zinc and are permanently in a damp, unrinsed, unlit gap. On the harbour side that is where a flashing usually fails first, and it is entirely invisible until somebody lifts a tile.

When the flashing has gone but the window has not

This is a common and slightly awkward position. A twenty-year-old skylight with sound timber, a clear sealed unit and a hinge that still holds, sitting inside a flashing perimeter that has perforated. The metal has to come off, which means the tiles round it come off, which is most of the labour of a replacement anyway.

The honest arithmetic is that re-flashing alone makes sense when the unit has real life left and the covering will lift cleanly. Where the window is within a few years of its own end, or the tiles are brittle, doing it twice costs more than doing it once. We will give you both numbers after the survey rather than steering you.

Salt on the harbour side and what it does to VELUX flashing zinc
A prepared kerb, squared and weatherproofed, before the unit goes on.

Inspection, and what we actually look at

  1. From the cleaning position, the head section and the top corners, where wind-driven salt collects and rain does not rinse.
  2. The apron and the tile course immediately below it, for lifted laps and for staining running down the covering.
  3. Every visible fixing, for rings and for rust bleed.
  4. The side sections at the point where they pass under the covering, for pitting at the waterline.
  5. Where accessible, one soaker lifted to see what the hidden zinc is doing.
  6. The frame drainage and the gap behind the apron, for salt crystal and for sand, which on the spit arrives in quantity.

What we specify, by zone

We are an independent installer with no accreditation, approval or partner status with VELUX or any other manufacturer.

Within sight of open water, that means a coated flashing, stainless fixings throughout, a washed perimeter twice a year and a six-monthly look. On a Canford Heath or Broadstone rooflight the same window goes in with the standard kit and an annual glance, and we say so, because recommending marine-grade hardware on a sheltered heathland roof is selling you something the weather will never test.

If you want a view on what is on your roof now, send a photograph of the flashing perimeter to 447880284133 on WhatsApp, or call 01202 923272. Our own workmanship carries a ten-year guarantee, given directly by us and not insurance backed, with a fixed written price after survey.

Get a fixed quote

Get a fixed quote

Tell us which way your roof faces.

We will come back with a specification, not a catalogue page. If your extension faces south we will tell you the G-value we would fit and why.

  • No pressure, no doorstep sales call
  • We handle the Building Control notification
  • 10-year workmanship guarantee on every installation
  • Installations and replacements across Poole and south Dorset

Prefer to talk it through? 01202 923272